4.45V LCO
PE
Graphite
Electrolyte
LCO
Cathode Powder
15.5um
0.20m2/G
2.5g/cm3
186 mAh/G
≥94.0%
Gelon
Export Stanard Package
lCO 4.45V
China(Mainland)
Product Description
High Voltage 4.45V LCO Battery Cathode Powder with 186 mAh/g Capacity for Lithium Ion Batteries
1. Purpose and scope of application
Lithium-ion battery cathode material, used in various liquid lithium-ion batteries .
2. Material type and model
2.1 Product Type: Lithium Ion Battery Cathode Material - Lithium Cobalt Oxide
2.2 Product model: L802F
2.3 Product voltage adaptation range: 3.0~4.45V
1. Purpose and scope of application
Lithium-ion battery cathode material, used in various liquid lithium-ion batteries .
2. Material type and model
2.1 Product Type: Lithium Ion Battery Cathode Material - Lithium Cobalt Oxide
2.2 Product model: L802F
2.3 Product voltage adaptation range: 3.0~4.45V
Item | Unit | Standard | Test Method | |
Chemical Compositions | Li | % | 7.1±0.3 | ICP |
Co | % | 60.0±2.0 | ICP | |
Impurity | Fe | ppm | ≤0.0050 | ICP |
Ni | ppm | ≤100 | ICP | |
Na | ppm | ≤100 | ICP | |
Cu | ppm | ≤0.020 | ICP | |
Particle Size Distribution | D10 | μm | 3.75±1.25 | Laser particle size detector |
D50 | μm | 15.5±1.5 | Laser particle size detector | |
D90 | μm | 30.0±5.0 | Laser particle size detector | |
D99 | μm | ≤55 | Laser particle size detector | |
pH | / | 9.80 | PH | |
Moisture | ppm | ≤0.02 | Coulomb Karl Fischer moisture tester | |
BET Surface Area | m2/g | 0.20±0.10 | Gas adsorption method | |
Tap Density | g/cm3 | ≥2.5 | Vibration-Density tester | |
1st Discharge Capacity (CR2032, 0.1C, 3.0 ~ 4.5V v.s. Li) | mAh/g | ≥186 mAh/g | ||
1st efficiency | % | ≥94.0 |