Cautop Vehicle & Parts

FAW L4bh 15-20ton Hydrochloric Acid Sulfuric Acid Tanker Transport Truck (14500Liters Q235 Steel Tank Lined LDPE 18-20mm), Hydrochloric Acid Tanker, Sulfuric Acid Tanker

Supplier Hubei Dong Runze Special Vehicle Equipment Co., Ltd.
Price $ 16880.00 / Piece
Availability In Stock
Mini Order: 1   Piece
Purchase details
Payments:
Tax:
Tax Included
Returns & Refunds:
Eligible for refunds within 30 days of receiving products. returns and refunds

Product detail

Model NO.
FAW Sulfuric Acid Tanker
Tank Volume
14500L
Drive Wheel
6×2
Horsepower
251-350hp
Engine Capacity
>8L
Storage
Chemical
Tire Certification
ISO, DOT
Tire Design
Radial
Condition
New
Tank Material
Carbon Steel Lined PE
Steel Shell Thickness
5mm-6mm
Lined
16-18mm LLDPE
Tank Net Weight
5500-6000kg
Overall Size
9000X2500X3550
Chassis
FAW Ca1260pk
Transport Package
Nil
Specification
5260GFWCA6
Trademark
DRZE
Origin
China
HS Code
8705909990
Production Capacity
10000
After-sales Service:
24hours
Warranty:
1 Year
Transmission Type:
Manual
Power:
Diesel
Load Capacity:
11-20t
Emission Standard:
Euro 3- 6
FAW L4BH 15-20Ton Hydrochloric Acid Sulfuric Acid Tanker Transport Truck ( 14500Liters  Q235 Steel Tank Lined LDPE 18-20mm)

Customizing Hydrochloric Acid Transporter Tanker (Truck To Carry HCL Steel Lined LLDPE Tank 14500Liters Without Chassis)
 


  Hydrochloric Acid Tanker Lorry Truck  18500Liters Carbon Steel Lined 16mm PE Tank, Chassis Mounted SKD Chemical Tank Body 
 Acid oil tanker truck for HCL, NaCIO acid Tank hydrochloric acid -HCL, dilute sulphuric acid WEAK SULFURIC ACID -H2SO4 ,sodium hypochlorite - NaCIO ,Caustic soda-NaOH
 
  




 
 

transport media   name: hydrochloride, hydrogen chlorate, sodium hydroxide,

acrylic (media   density are for 1190 kilograms/cubic metres),

acetic acid,   glacial acetic acid, hydrogen peroxide (media density are for 1140   kilograms/cubic metres)

Propionic acid, (density for   1110 kilograms/cubic metres),

ammonia, (NH3·H2Odensity for 1090 kilograms/cubic metres), 

Hydrochloric acid  tank 

 
 FAW  Chassis optional LHD RHD   
 
PlatformEmission Model NumberSteering WheelOriginal Exporting CountryEngine Manufacturer And ModelEngine PowerGearbox Manufacturer And Model 
Power Take-off 
PTO
TyreWheelbase
J5KEuro 1CA1122PK2L2Y  Xichai CA6110 / 125Z120PSFAW ca6tbx085m10.00r2016 level4770
New VenusEuro 2CA3256P2K2T1EA81LHDCote d'IvoireWeichai wp10.340e32340PSShaanxi gear 9jsd135t12r22.5-18pr level3825+1350
New VenusEuro 2CA3256P2K2T1EYA81RHDQingdao heavy industry - MozambiqueWeichai wp10.340e32340PSShaanxi gear rtd-11509c12.00r2018 level3700+1350
New VenusEuro 2CA3256P2K2T1EA81LHDNigeriaWeichai wp10.340e32340PSShaanxi gear rtd-11509c12.00r2018 level3825+1350
New VenusEuro 2CA3256P2K2T1EYA81RHDKenyaWeichai wp10.340e32340PSShaanxi gear rtd-11509c315/80R22.5-203700+1350
New VenusEuro 2CA3256P2K2T1EYA80RHDBengalWeichai wp10.340e32340PSShaanxi gear 9jsd135t11.00r2016 level3500+1350
New VenusEuro 2CA3256P2K2T1EA80RHDdominicaWeichai wp10.340e32340PSShaanxi gear 9jsd135t12.00R20183700+1350
New VenusEuro 2CA3256P2K2T1EA81RHDPakistanWeichai wp10.340e32340PSShaanxi gear 9jsd135t12.00r2018 level4400+1350
New VenusEuro 2CA3256P2K2T1EA81RHDPakistanWeichai wp10.340e32340PSShaanxi gear 9jsd135t12.00r2018 level4400+1350
New VenusEuro 2CA3256P2K2T1EA80LHDEgyptWeichai wp10.380e32380PSShaanxi gear 12jsd160t12.00r2418 level3650+1450
New VenusEuro 2CA3256P2K2T1EA80RHDAntiguaWeichai wp10.380e32380PSEaton et-20113315 / 80r22.5-20pr level3700+1350
New VenusEuro 2CA3256P2K2T1EA81RHDMalawiWeichai wp10.380e32380PSShaanxi gear 12jsd160ta12.00r2018 level3825+1350
New VenusEuro 2CA3256P2K2T1EA80LHDGhanaWeichai wp10.380e32380PSShaanxi gear 12jsd160t13r22.5-18pr level3700+1350
New VenusEuro 2CA3256P2K2T1EA81LHDRwandaWeichai wp10.380e32380PSShaanxi gear 12jsd160t315 / 80r22.5-20pr level3700+1350
New VenusEuro 2CA1252P2K2T1YA80RHDTrinidadWeichai wp10.380e32380PSEaton et-2011312r22.5-18pr level4600+1350
New VenusEuro 3CA3256P2K2T1EA81LHDSaudi ArabiaXichai ca6dl2-35e3350PSEaton eto-20109a315 / 80r22.5-20pr level5200+1350
New VenusEuro 3CA3256P2K2T1EYA80RHDThailand-sXichai ca6dm2-37e3370PSEaton et-20109a295 / 80R22.5 level4150+1350
New VenusEuro 3CA3256P2K2T1EYA80RHDThailand-sXichai ca6dm2-37e3370PSEaton et-20109a295 / 80R22.5 level4150+1350
New VenusEuro 3CA3256P2K2T1EA81LHDPeruWeichai wp12.375n380PSEaton eto-2011312.00r2018 level3700+1350
New VenusEuro 3CA3256P2K15T1EYA80RHDThailand-aWeichai wp12.375n375PSEaton eto-20109a11.00R20184150+1350
New VenusEuro 3CA3256P2K2T1EA81LHDPeruWeichai wp12.430n430PSZF16S2230 TO12.00r2018 level3700+1350
New VenusEuro 5CA3256P2K15T1NA80LHDColumbiaWeichai wp12ng380e51380PSEaton eto-2011312.00r2018 level4300+1350
New VenusEuro 2CA3310P2K2T4EYA80RHDSouth AfricaWeichai wp10.340e32340PSFAW ca9tb160m315 / 80r22.5-18pr level1900+3400+1350
New VenusEuro 2CA3312P2K2L4T4EA80RHDPakistanWeichai wp10.340e32340PSShaanxi gear 9jsd135t12.00r2018 level1860+3960+1350
New VenusEuro 2CA3312P2K2L4T4EA80LHDthe PhilippinesWeichai wp10.340e32340PSShaanxi gear 12jsd160t12.00r2018 level1860+3960+1350
New VenusEuro 2CA3312P2K2L4T4EYA80RHDTanzaniaWeichai wp10.380e32380PSShaanxi gear 12jsd160t315 / 80r22.5-20pr level1860+3960+1350
New VenusEuro 2CA3312P2K2L4T4EA80LHDMaliWeichai wp10.380e32380PSShaanxi gear 12jsd160t12.00r2018 level1860+3960+1350
New VenusEuro 2CA3312P2K2L4T4EA80RHDIndonesiaWeichai wp10.380e32380PSFAW ca9tb160m12.00r2420 level1860+3910+1450
New VenusEuro 2CA3312P2K2L4T4EA80LHDGhanaWeichai wp10.380e32380PSShaanxi gear 12jsd160t13r22.5-18pr level1860+3960+1350
New VenusEuro 2CA3312P2K2L4T4EA80LHDDRCWeichai wp10.380e32380PSShaanxi gear 12jsd160t12.00r2418 level1860+3910+1350
New VenusEuro 2CA3312P2K2L4T4EA80LHDCongoWeichai wp10.380e32380PSShaanxi gear 12jsd160t12.00r2018 level1860+3960+1350
New VenusEuro 2CA3312P2K2L4T4EA80RHDIndonesiaWeichai wp10.380e32380PSFAW ca9tb160m12.00r2418 level1860+3910+1350
New VenusEuro 2CA3312P2K2L5T4EA80LHDboliviaWeichai wp12.380e32380PSShaanxi gear 12jsd160t12.00r2018 level1860+4360+1350
New VenusEuro 2CA3312P2K2L4T4EA80LHDthe PhilippinesWeichai wp12.380e32380PSShaanxi gear 12jsd160t12.00r2018 level1860+3700+1350
New VenusEuro 2CA1310P2K2L7T4YA80RHDMalaysiaXichai CA6DM2-42420PSEaton et-20109a295/80R22.5-181860+5660+1350
New VenusEuro 2CA3312P2K2L4T4EA80LHDGhanaWeichai wp12.420e32420PSShaanxi gear 12jsd200t13r22.5-18pr level1860+3700+1350
New VenusEuro 5CA3310P2K15L4T4NA80LHDArmeniaWeichai wp12ng380e51380PSShaanxi gear 12jsd180ta12r22.5-18pr level1860+3960+1350
New VenusEuro 5CA3310P2K15L4T4NA80LHDArmeniaWeichai wp12ng380e51380PsEaton et-20109a12r22.5-18pr level1860+3960+1350
New VenusEuro 5CA3310P2K15L4T4NA80LHDArmeniaWeichai wp12ng380e51380PSShaanxi gear 12jsd180ta12r22.5-18pr level1860+3960+1350
JH6Euro 3CA3250P25K15T1EA80LHDPhilippines qsjWeichai wp12.375n375PSShaanxi gear 12jsd180ta12.00r2018 level3800+1350
JH6Euro 5CA3250P25K15L3T1E5A80LHDthe PhilippinesWeichai wp10h375e50375PSShaanxi gear 12jsd180t12.00R20163800+1350
JH6Euro 5CA3250P25K15L3T1E5A80LHDthe PhilippinesWeichai wp10h375e50375PSShaanxi gear 12jsd180ta12.00r2016 level3800+1350
JH6Euro 5CA3250P25K15L3T1E5A80LHDChileXichai ca6dm2-42e52420PSShaanxi gear 12jsdx240ta13r22.5-18pr level3900+1350
JH6Euro 5CA3250P25K15L3T1E5A80LHDChileXichai ca6dm2-42e52420PSShaanxi gear 12jsdx240ta13r22.5-18pr level3900+1350
JH6Euro 5CA3310P25K15L3T4E5A80LHDChileXichai ca6dm2-42e52420PSShaanxi gear 12jsdx240ta13r22.5-18pr level1900+3400+1350
JH6Euro 5CA3310P25K15L3T4E5A80LHDChileXichai ca6dm2-42e52420PSShaanxi gear 12jsdx240ta13r22.5-18pr level1900+3400+1350
JH6Euro 5CA3310P25K15L3T4E5A80LHDthe PhilippinesWeichai wp12.430e50430PSShaanxi gear 12jsdx240ta12.00r2018 level1900+3800+1350
JH6Euro 5CA3310P25K15L3T4E5A80LHDAzerbaijanWeichai wp12.430e50430PSShaanxi gear 12jsdx240ta12.00r2018 level1900+3400+1350
J5KEuro 2CA5121PK2L2YA80RHDUgandaXichai ca6df2d-18180PSFAW ca6tbx075m10.00R20164180
J5MEuro 2CA1250P1K2L3T1EYA80RHDBengalWeichai wp6.240e32240PSShaanxi gear 8js118t10.00r2016 level4615+1350
J5MEuro 2CA1253P7K2L7T1YA80RHDMalaysiaXichai ca6dl1-28280PSEaton et-16109a295 / 80R22.5 level6500+1350
Fierce VEuro 2CA5161XXYPK2L5EA80-3LHDKoreaXichai ca6df2d-22220PSShaanxi gear 8js85e10.00r2016 level6100
Fierce VEuro 5CA1180P1K2L3E5A80LHDChileXichai ca6dld-22e5220PSShaanxi gear 8js118tc295 / 80r22.5-18 level4770
Fierce VEuro 5CA1180P1K2L5E5A80-1LHDChileXichai ca6dld-22e5220PsShaanxi gear 8js118tc295 / 80R22.5 level5600
Dragon VEuro 5CA1160P40K2L3E5A85LHDKazakhstanWeichai wp4.6nq220e50220PSShaanxi gear 8js85tc9.00R20164200
Day VEuro 2CA5250GJBEA80LHDParaguay Luliang HuanyouWeichai wp10.380e32380PSShaanxi gear 12jsd160t12.00R20183800+1350
Day VEuro 3CA5340P2K2L5T1BE5A80LHDCambodia - Jiuhe heavy industryXichai ca6dm2-42e3420PSShaanxi gear 12jsd200ta12.00r2020 level4700+1350
Day VEuro 5CA5250GJBE5A80LHDthe PhilippinesWeichai wp10.350e53350PSShaanxi gear 12jsd160ta12.00r2018 level4000+1350
Day VEuro 5CA5310GJBNA80LHDUzbekistanWeichai wp12ng380e51380PSShaanxi gear 12jsd180ta315 / 80r22.5-20pr level1860+3960+1350
Day VEuro 5CA5310GJBNA80LHDMexico-eWeichai wp12ng400e50400PSShaanxi gear 12jsd180ta12.00r2018 level1860+3600+1350
New VenusEuro 2CA5253GJBEA80LHDthe PhilippinesWeichai wp10.270e32270PSShaanxi gear 9js119t10.00r2016 level3500+1350
New VenusEuro 2CA1250P2K2L3T1EA80RHDPakistanWeichai wp10.340e32340PSShaanxi gear 9jsd135t12.00r2018 level4400+1350
New VenusEuro 2CA5250GJBEA80LHDthe PhilippinesWeichai wp10.340e32340PSShaanxi gear rtd-11509c12.00r2018 level4000+1350
New VenusEuro 2CA5256P2K2T1EYA80RHDBengalWeichai wp10.340e32340PSShaanxi gear 9jsd135t12.00r2018 level4600+1350
New VenusEuro 2CA1250P2K2T1S2EYA80RHDSouth AfricaWeichai wp10.340e32340PSFAW ca9tb160m315 / 80r22.5-18pr level3500+1350
New VenusEuro 2CA5250GJBEYA80RHDBengalWeichai wp10.340e32340PSShaanxi gear 9jsd135t11.00r2016 level3400+1350
New VenusEuro 2CA5250GJBEA80RHDdominicaWeichai wp10.340e32340PSShaanxi gear 9jsd135t12.00R20183400+1350
New VenusEuro 2CA5256P2K2L3T1EA80LHDLiberiaWeichai wp10.380e32380PSShaanxi gear 12jsd160t13r22.5-18pr level4600+1350
New VenusEuro 2CA5250GJBEA80LHDIraq Qingdao heavy industryWeichai wp10.380e32380PSShaanxi gear 12jsd160t12R22.5-183800+1350
New VenusEuro 2CA5250GJBYA80RHDMalaysiaXichai ca6dm2-39390PsEaton et-20109a295 / 80R22.5 level4150+1350
New VenusEuro 2CA5250GJBYA80RHDMalaysiaXichai ca6dm2-39390PSEaton et-20109a295 / 80R22.5 level6500+1350
New VenusEuro 2CA5250GJBYA80RHDMalaysiaXichai CA6DM2-42420PSEaton et-20109a295 / 80R22.5 level4150+1350
New VenusEuro 3CA5250GJBEA80RHDThailand-aWeichai wp10.336n340PSFAW ca9tbx180m12r22.5-18pr level3400+1350
New VenusEuro 3CA5250GJBEA80RHDThailand-aWeichai wp10.336n340PSFAW ca9tbx180m11.00r2016 level3400+1350
New VenusEuro 3CA5250P2K15L4T1EA80LHDThailand-aWeichai wp12.375n375PSEaton eto-20109a11.00r2018 level5100+1350
New VenusEuro 5CA5250GJBNA80LHDArmeniaWeichai wp12ng380e51380PSShaanxi gear 12jsd180ta12.00r2018 level4850+1350
New VenusEuro 5CA5250GJBNA80LHDArmeniaWeichai wp12ng380e51380PSShaanxi gear 12jsd180ta12.00r2018 level4560+1350
New VenusEuro 2CA1310P2K2T4S2EYA80RHDSouth AfricaWeichai wp10.340e32340PSFAW ca9tb160m315/80R22.5-181900+3400+1350
New VenusEuro 2CA5310GJBEA80LHDEgyptWeichai wp10.380e32380PSShaanxi gear 12jsd160t12.00r2420 level1860+3260+1350
New VenusEuro 2CA5310GJBYA80RHDMalaysiaXichai ca6dm2-39390PSEaton et-20109a295 / 80R22.5 level1860+4000+1350
New VenusEuro 5CA5310GJBNA80LHDUzbekistanWeichai wp12ng380e51380PSShaanxi gear 12jsd180ta315 / 80r22.5-20pr level1860+3960+1350
JH6Euro 3CA5250GJBP25K2L1T1EA80LHDEcuadorWeichai wp12.375n375PSShaanxi gear 12jsd180ta12r22.5-18pr level3900+1350
JH6Euro 5CA1250P25K2L2T1S2E5A80LHDPhilippines qsjWeichai wp10h375e50375PSShaanxi gear 12jsd180ta12.00R20164000+1350
JH6Euro 5CA5251P25K15L4T1E5A80LHDChileXichai ca6dm2-42e52420PSShaanxi gear 12jsdx240ta13r22.5-18pr level4800+1350
JH6Euro 5CA5250P25K15L3T1E5A80LHDChileXichai ca6dm2-42e52420PSShaanxi gear 12jsdx240ta13r22.5-18pr level3900+1350
JH6Euro 5CA5310P25K15L3T4E5A80LHDChileXichai ca6dm2-42e52420PSShaanxi gear 12jsdx240ta13r22.5-18pr level1900+3400+1350

Our  water tank truck with different chassis, eg:DFAC, DFL, SINOTRUCK, CNHTC,NORTH BENS, FOTON, Qingling, JAC, JMC, KAMA, YUEJIN, etc.
 
Rotationally Molded LLDPE TANK
 
 
 cautop.com/store/tictrucks   

LDPE / HDPE Chemical Resistance Chart 

The chemical compatibility of LDPE and HDPE on this chart is tested at 20°C: and 50°C: for 7 days and 30 days (if applicable) with constant exposure.

LDPE & HDPE resistance listed by chemical
1.4-dioxaneLDPE / HDPE at 20°C: little or no damage after 30 days.
LDPE at 50°C: shows some effect after 7 days.
AcetaldehydeLDPE / HDPE at 20°C: little or no damage after 30 days.
HDPE at 50°C: shows some effect after 7 days.
LDPE at 50°C: immediate damage may occur.
Acetic Acid 5 %LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Acetic Acid, glacial 50%LDPE / HDPE at 20°C: little or no damage after 30 days.
LDPE at 50 °C: immediate damage may occur.
AcetoneLDPE / HDPE at 20°C-50°C: damage may occur.
Not recommended for continuous use.
Allyl AlcoholLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Aluminum saltsLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Amino acidsLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
AmmoniaLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Ammonium carbonate saturatedLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Ammonium phosphateLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Ammonium sulphateLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Amyl chlorideHDPE at 20°C: shows some effect after 7 days.
HDPE at 50°C & LDPE at 20°C-50°C: immediate damage may occur.
Not recommended for continuous use.
AnilineLDPE / HDPE at 20°C: little or no damage after 30 days.
HDPE at 50°C: shows some effect after 7 days.
BenzeneLDPE / HDPE at 20°C-50°C: damage may occur.
Not recommended for continuous use.
Benzyl alcoholLDPE / HDPE at 50°C: immediate damage may occur.
HDPE at 20°C: shows some effect after 7 days.
Boric acidLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
BromineLDPE / HDPE at 50°C: immediate damage may occur.
HDPE at 20°C: shows some effect after 7 days.
Butyric acidLDPE / HDPE at 50°C: immediate damage may occur.
HDPE at 20°C: shows some effect after 7 days.
Calcium chlorideLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Calcium hydroxide saturatedLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Carbon tetrachlorideHDPE at 20°C: shows little or no damage after 30 days.
LDPE at 20°C & HDPE at 50°C: show some effect after 7 days.
LDPE at 50°C: not recommended.
Chlorine 10% in waterLDPE / HDPE at 20°C: shows little or no damage after 30 days.
LDPE at 50°C: shows damage and is not recommended.
ChlorobenzeneImmediate damage may occur.
Not recommended for continuous use.
ChloroformLDPE / HDPE at 20°C: show some effect after 7 days.
LDPE / HDPE at 50°C: immediate damage may occur.
Not recommended for continuous use.
Chromic acid 10%LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Chromic acid 50%LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Citric acid 10%LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
CresolHDPE at 20°C: shows some effect after 7 days.
LDPE at 20°C-50°C & HDPE at 50°C: show immediate damage.
Not recommended for continuous use.
CyclohexaneLDPE / HDPE at 50°C: immediate damage may occur.
LDPE / HDPE at 20°C: show some effect after 7 days.
Diethyl ketoneLDPE / HDPE at 20°C-50°C: damage may occur.
Not recommended for continuous use.
DimethylsulfoxideLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Ethanol 95%LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Ethyl acetateLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Ethyl benzeneHDPE at 20°C: shows some effect after 7 days.
LDPE at 20°C-50°C & HDPE at 50°C: show immediate damage.
Not recommended for continuous use.
Ethylene glycolLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Ethylene oxideHDPE at 20°C: shows little or no damage after 30 days.
LDPE at 20°C: and LDPE/ HDPE at 50°C: show some effect after 7 days.
Ferric chlorideLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
FluorideLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
FluorineHDPE at 20°C: shows little or no damage after 30 days.
LDPE at 20°C: shows some effect after 7 days.
Not recommended at 50°C.
Formaldehyde 10%LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Formaldehyde 40%LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
GlycerolLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
HexaneHDPE at 20°C: shows little or no damage after 30 days continuous use.
HDPE at 50 °C: shows some effect after 7 days.
LDPE not recommended at any temperature.
Hydrochloric acid 20%LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Hydrochloric acid 35%LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Hydrochloric acid 5%LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Hydrocyanic acidLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Hydrofluoric acidLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Hydrofluoric acid 4%LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Hydrofluoric acid 48%LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Hydrogen peroxide 3%LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Hydrogen peroxide 30%LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Isobutyl alcoholLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Isopropyl alcoholLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
KeroseneLDPE / HDPE at 20°C: show some effect after 7 days.
LDPE / HDPE not recommended at 50°C, as immediate damage may occur.
Lactic Acid 10 %LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Lactic Acid 90 %LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Lead acetateLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
MethanolLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Methyl ethyl ketoneImmediate damage may occur.
Not recommended for continuous use.
Methyl propyl ketoneHDPE at 20°C: shows some effect after 7 days.
LDPE at 20°C-50°C & HDPE at 50°C: Immediate damage may occur.
Not recommended for continuous use.
Methylene chlorideHDPE at 20°C: shows some effect after 7 days.
LDPE at 20°C-50°C & HDPE at 50°C: Immediate damage may occur.
Not recommended for continuous use.
Mineral oilLDPE / HDPE at 20°C: little or no damage after 30 days.
LDPE at 50°C: may show immediate damage and is not recommended.
n-amyl acetateLDPE / HDPE at 20°C: little or no damage after 30 days.
LDPE at 50°C: shows some effect after 7 days or constant exposure.
n-butyl alcoholLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Nitric acid 50 %LDPE at 20°C: shows little or damage after 30 days.
HDPE at 20°C & LDPE at 50°C: show effect after 7 days.
HDPE at 50°C: shows immediate damage and is not recommended.
Nitric acid 70 %LDPE / HDPE at 20°C: show some effect after 7 days.
LDPE / HDPE at 50°C: show immediate damage.
Not recommended.
n-octaneLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Oleic acidHDPE at 20°C-50°C: little or no damage after 30 days.
LDPE at 20°C-50°C: shows immediate damage and is not recommended.
Oxalic acidLDPE at 20°C: shows some effect after 7 days.
HDPE at 20°C and LDPE / HDPE at 50°C: shows little/ no damage after 30 days.
OzoneLDPE / HDPE at 20°C: little or no damage after 30 days.
LDPE / HDPE at 50°C: show immediate damage.
Not recommended.
Perchloric acidLDPE / HDPE at 20°C: little or no damage after 30 days.
LDPE / HDPE at 50°C: show immediate damage.
Not recommended.
Perchloric ethyleneLDPE / HDPE at 20°C-50°C: show immediate damage.
Not recommended.
PhenolLDPE / HDPE at 20°C-50°C: show immediate damage.
Not recommended.
Phosphoric acid 10%LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Phosphoric acid 85%LDPE / HDPE at 20°C: little or no damage after 30 days.
LDPE at 50°C: shows immediate damage and is not recommended.
Phosphorous trichlorideLDPE / HDPE at 20°C: little or no damage after 30 days.
LDPE at 50°C: has no data available. HDPE at 50°C: shows some effect after 7 days.
Potassium carbonateLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Potassium hydroxide 5 %LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Potassium hydroxide concentratedLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Potassium permanganateLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Propylene glycolLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
PyridineImmediate damage may occur.
Not recommended for continuous use.
Salicylic acid, saturatedLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Silver acetateLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Silver nitrateLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Sodium carbonateLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Sodium chloride, saturatedLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Sodium dichromateLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Sodium hydroxide 1%LDPE at 20°C-50°C: shows little or no damage after 30 days.
HDPE at 20°C-50°C: shows some effect after 7 days.
Sodium hydroxide 50%LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Sodium hypochlorite 15%HDPE at 20°C-50°C: little or no damage after 30 days.
LDPE at 20°C: is suitable
 but at 50°C: shows some effect after 7 days.
Sodium nitrateLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Sodium sulphateLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
SucroseLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Sulfuric acid 20%LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Sulfuric acid 6%LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Sulfuric acid 60%LDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
Sulfuric acid 98%LDPE at 20°C-50°C: shows little or no damage after 30 days.
HDPE at 20°C: shows effect after 7 days.
Not recommended for use at 50°C.
Tannic acidLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
TetrahydrofuranLDPE / HDPE at 20°C: show some effect after 7 day of constant exposure.
LDPE / HDPE at 50°C: show immediate damage.
Not recommended.
TolueneLDPE at 20°C: show some effect after 7 day of constant exposure.
HDPE at 20°C-50°C & LDPE at 50°C: show immediate damage.
Not recommended.
Trichloracetic acidLDPE / HDPE at 20°C: show some effect after 7 day of constant exposure.
LDPE / HDPE at 50°C: show immediate damage.
Not recommended.
TrichlorethaneImmediate damage may occur.
Not recommended for continuous use.
Turpentine oilLDPE / HDPE at 20°C: show some effect after 7 days.
LDPE / HDPE at 50°C: show immediate damage.
Not recommended.
UreaLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.
XyleneHDPE at 20°C: shows some effect after 7 day of constant exposure.
LDPE at 20-50°C and HDPE at 50°C: show immediate damage.
Not recommended.
Zinc chlorideLDPE / HDPE at 20°C-50°C: little or no damage after 30 days.